    Looking for a plastic/ceramic material USDA approved.

    Attached is the application, the friction or need of lubrication between the plastic/ceramic and the stainless is not nessecary also the movment is very slow maybe 6.0ft/min. We used Ultem and it is failing due to the chemical concentration of chlorine solution used to clean the machine. We...
  2. S

    Looking for a plastic/ceramic material USDA approved.

    I have been looking for hours tring to find a material with these properties. Working Temperature up to 500° F Low coefiecient of Friction Chemical Resistance to Costic Cleaners (mainly chlorinated) Coeffecient of Thermal Expansion around 9.5 μin/in°F decent machine ability made in 1/4"...