Dissolving Zr and Y in nitric acid

  • Thread starter Thread starter Bakery87
  • Start date Start date
  • Tags Tags
    Acid
AI Thread Summary
Concentrated nitric acid (~70%) is being considered for dissolving zirconium (Zr) and yttrium (Y) metals, with a focus on maintaining high metal molarity in the solution while avoiding overheating. The dissolution rate is influenced by the surface area of the metals; finely divided powders dissolve faster than larger pieces. The user seeks to avoid using metal powder due to the violent reaction it can cause in nitric acid. A calculation suggests a 4 M H+/1 M metal ratio for the dissolution process. However, it has been noted that zirconium cannot be effectively dissolved in nitric acid, hydrochloric acid, or similar acids. Alternatives such as hydrofluoric acid or a mixture of sulfuric and hydrochloric acids may be more effective, but there are conflicting reports regarding the dissolution of zirconium based on its preparation. Additionally, the user is interested in methods for producing zirconyl nitrate from the metal.
Bakery87
Messages
10
Reaction score
0
Hey all,

I have concentrated nitric acid (~70%), and I want to use it to dissolve Zr/Y metal. I've dissolved Y before, and I know it's as simple as putting metal into acid. The question I have, is there a known dissolution rate I should use to barely dissolve the metals in the acid? I wish to keep my metal molarity as high as possible in the finished solution. I also would like to avoid overheating of my mixture if possible. I know using concentrated acids can be tricky.

Any help would be appreciated.

M
 
Chemistry news on Phys.org
Dissolution rate is strongly dependent on the surface area of the metals. Finely divided powders dissolve much more rapidly than shavings which dissolve much faster than briquettes or large lumps of metal. There is no way to answer your question without more information.
 
That would make the time shorter, which I don't care about. I can grind down a sample of my Zr chunks into a powder type form, but I am trying to avoid powder. Dissolving metal powder in nitric acid is violent, so I was hoping to just be able to calculate the minimum amount of acid to dissolve X grams Zr and Y grams Y.

I calculate it should be about a 4 M H+/ 1 M metal total, but what is the best way to add the acid to the metal? Add all of the metal to a beaker and then slowly add the measured amount of acid, or ...?
 
So, as it turns out, one can not dissolve Zr in nitric acid, hydrochloric, or others. HF seems to be the route, or possibly a mixture of H2SO4/HCl or perchloric acid. There are many conflicting reports on the subject. It appears to be related to how the Zr was prepared in the first place.

If I could find out how to make zirconyl nitrate from the metal, that would also be very helpful, and I plan on making another post on the subject.
 
Thread 'How to make Sodium Chlorate by Electrolysis of salt water?'
I have a power supply for electrolysis of salt water brine, variable 3v to 6v up to 30 amps. Cathode is stainless steel, anode is carbon rods. Carbon rod surface area 42" sq. the Stainless steel cathode should be 21" sq. Salt is pure 100% salt dissolved into distilled water. I have been making saturated salt wrong. Today I learn saturated salt is, dissolve pure salt into 150°f water cool to 100°f pour into the 2 gallon brine tank. I find conflicting information about brine tank...
Engineers slash iridium use in electrolyzer catalyst by 80%, boosting path to affordable green hydrogen https://news.rice.edu/news/2025/engineers-slash-iridium-use-electrolyzer-catalyst-80-boosting-path-affordable-green Ruthenium is also fairly expensive (a year ago it was about $490/ troy oz, but has nearly doubled in price over the past year, now about $910/ troy oz). I tracks prices of Pt, Pd, Ru, Ir and Ru. Of the 5 metals, rhodium (Rh) is the most expensive. A year ago, Rh and Ir...
Back
Top